Hi friends, I am Alexander Mahonin, head of the Nika construction company. Today I want to bring to your attention
Video instructions for performing coating waterproofing with mastic. We will use Technonicol mg mt-24 mastic
We take out the cones, clean up the concrete inflows with a perforator,
we cover all the holes with technological waterproofing with a rigid cement-based coating - Ceresit, granite, any companies.
We also cover up all the shells that we have, especially at the bottom, this is very important.
Next, we take the number one bitumen-based primer from Technonicol. He will be the ground for us.
But now we apply a primer with a roller or brush, respectively, we do not regret it, we spread it abundantly and do not roll it out, do not dry it.
Do not rush, if your holes are sealed and have not had time to dry yet, skip them.
You still have time to cover them up before applying the main waterproofing itself.
The first layer was applied, now the temperature is 24 degrees per sol
The first layer has already been absorbed by concrete in just half an hour, so now we are applying the second layer, the guys have already started applying it from the other side.
Therefore, at the end of the work I will give expenses. Technonicol according to the technical description says the consumption will be 350 grams per square meter. Well, I'll tell you later in reality how much we will show at this temperature.
Let's go apply waterproofing. In general, it can be applied with a spatula, it turns out that the layer is more thick with a millimeter thick.
We are already planning to install insulation tomorrow.
And of course the mastics on our square. our house turns out to be 3.30 m high, the basement is more precisely, not a house, but a basement with a height of 3.30 and, accordingly, it is 9 by 12.5 meters.
We missed the connection, remember the waterproofing is rigid and we also missed this corner abundantly with waterproofing, in addition to it, there is also a waterproofing tape in the reinforced concrete slab structure.
This node is our corner cold seam, of course the most vulnerable, so we try to waterproofing it as much as possible.
Here is such a client, I will also tell you later what it is called. When interacting with water and concrete, it expands and compacts in concrete. The seal is obtained. It fits when the formwork is exposed. The formwork is exposed, and it is laid in the middle and, accordingly, swells and fills the junction. fills, seals, seals the cold seam and water will not pass.
Friends, I am ready to provide you with the results.
Today is our third day.
The first layer has dried. Primer consumption. we have it at our volume of 330 milliliters per square meter, which in principle corresponds to the technical description. Verified
By the way, today we started to sticker insulation and fixing. There are also secrets, so go to the next video. Subscribe, like and be active. Thanks!
See the process of our work.

Пікірлер
  • Мастика заменяет наплавляемую рулонную гидроизоляцию? Дешевле получается?

    @user-el4vm4pe8y@user-el4vm4pe8y12 күн бұрын
  • А на уровне окон зачем наносите? Там же грунта не будет…

    @tymkoleg@tymkoleg7 ай бұрын
  • Где Ибрагим?

    @garzan1745@garzan174513 күн бұрын
KZhead